ISOMaterialsMaterial DesignationMaterial ConditionCutting Speed Recommendations (Vc)
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed :125100-300 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed :190100-300 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55%C.Quench and tempered. :250100-300 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55%C.Annealed :220100-300 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55%C.Quenched & tempered. :300100-300 m/min
P6Low alloy & cast steel (less than 5% of alloying elements).Annealed :200100-300 m/min
P7Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :275100-300 m/min
P8Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :300100-300 m/min
P9Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :350100-300 m/min
P10High alloyed steel, cast steel and tool steel.Annealed :200100-200 m/min
P11High alloyed steel, cast steel and tool steel.Quenched & tempered :325100-200 m/min
P12Stainless steel and cast steel.Ferritic/martensitic :200100-150 m/min
P13Stainless steel and cast steel.Martensitic :240100-150 m/min
M14Stainless steel and cast steel.Austenitic :180100-150 m/min
K15Grey cast iron (GG)Pearlitic/ferritic :180100-300 m/min
K16Grey cast iron (GG)Pearlitic/martensiti :260100-300 m/min
K17Nodular cast iron (GGG)Ferritic :16080-200 m/min
K18Nodular cast iron (GGG)Pearlitic :25080-200 m/min
K19Malleable cast iron.Ferritic :13080-200 m/min
K20Malleable cast iron.Pearlitic :23080-200 m/min
S31High temp. alloys Fe based.Annealed :20020-50 m/min
S32High temp. alloys Fe based.Cured :28020-50 m/min
S33High temp. alloys. Ni or Co based.Annealed :25020-50 m/min
S34High temp. alloys. Ni or Co based.Cured :35020-50 m/min
S35High temp. alloys. Ni or Co based.Castr :32020-50 m/min
S36Titanium Ti alloys.:31030-60 m/min
S37Titanium Ti alloys.Alpha+beta alloys cu :31030-60 m/min

Site Map:

External Turning  Internal Turning  Grooving & Parting  Threading  Milling  Holemaking  Boring  Tooling System 

Terms of Use and Legal Disclaimer   Privacy Statement   Privacy Settings
© 2024Tungaloy Corporation Manufacturer of Metalworking Tools (Tungaloy.co.jp) All Rights Reserved