ISO | Materials | Material Designation | Material Condition | Cutting Speed Recommendations (Vc) |
P | 1 | Non-alloy steel and cast steel, free cutting steel <0.25%C. | Annealed :125 | 160-250 m/min |
P | 2 | Non-alloy steel and cast steel, free cutting steel >=0.25%C. | Annealed :190 | 160-250 m/min |
P | 3 | Non-alloy steel and cast steel, free cutting steel <0.55%C. | Quench and tempered. :250 | 80-250 m/min |
P | 4 | Non-alloy steel and cast steel, free cutting steel >=0.55%C. | Annealed :220 | 80-250 m/min |
P | 5 | Non-alloy steel and cast steel, free cutting steel >=0.55%C. | Quenched & tempered. :300 | 80-250 m/min |
P | 6 | Low alloy & cast steel (less than 5% of alloying elements). | Annealed :200 | 160-250 m/min |
P | 7 | Low alloy & cast steel (less than 5% of alloying elements). | Quenched & tempered :275 | 160-250 m/min |
P | 8 | Low alloy & cast steel (less than 5% of alloying elements). | Quenched & tempered :300 | 80-200 m/min |
P | 9 | Low alloy & cast steel (less than 5% of alloying elements). | Quenched & tempered :350 | 80-200 m/min |
P | 10 | High alloyed steel, cast steel and tool steel. | Annealed :200 | 80-200 m/min |
P | 11 | High alloyed steel, cast steel and tool steel. | Quenched & tempered :325 | 80-200 m/min |
P | 12 | Stainless steel and cast steel. | Ferritic/martensitic :200 | 100-220 m/min |
P | 13 | Stainless steel and cast steel. | Martensitic :240 | 100-220 m/min |
M | 14 | Stainless steel and cast steel. | Austenitic :180 | 100-200 m/min |
S | 31 | High temp. alloys Fe based. | Annealed :200 | 20-60 m/min |
S | 32 | High temp. alloys Fe based. | Cured :280 | 20-60 m/min |
S | 33 | High temp. alloys. Ni or Co based. | Annealed :250 | 20-60 m/min |
S | 34 | High temp. alloys. Ni or Co based. | Cured :350 | 20-60 m/min |
S | 35 | High temp. alloys. Ni or Co based. | Castr :320 | 20-60 m/min |
S | 36 | Titanium Ti alloys. | :310 | 40-120 m/min |
S | 37 | Titanium Ti alloys. | Alpha+beta alloys cu :310 | 40-120 m/min |