ISO | Materials | Material Designation | Material Condition | Cutting Speed Recommendations (Vc) |
P | 12 | Stainless steel and cast steel. | Ferritic/martensitic :200 | 70-130 m/min |
P | 13 | Stainless steel and cast steel. | Martensitic :240 | 70-130 m/min |
M | 14 | Stainless steel and cast steel. | Austenitic :180 | 70-130 m/min |
S | 31 | High temp. alloys Fe based. | Annealed :200 | 20-80 m/min |
S | 32 | High temp. alloys Fe based. | Cured :280 | 20-80 m/min |
S | 33 | High temp. alloys. Ni or Co based. | Annealed :250 | 20-80 m/min |
S | 34 | High temp. alloys. Ni or Co based. | Cured :350 | 20-80 m/min |
S | 35 | High temp. alloys. Ni or Co based. | Castr :320 | 20-80 m/min |
S | 36 | Titanium Ti alloys. | :310 | 20-80 m/min |
S | 37 | Titanium Ti alloys. | Alpha+beta alloys cu :310 | 20-80 m/min |