Grade : AH9130 - Tungaloy Cutting Tools - Metal Working Tools
EN
×
 
 

Grade : AH9130

High wear resistance. Grade for drilling that can machining various materials.

PropertyValue
ISO Range - P/M/K(P15-P35)(M25-M35)(K10-K25)
ISO Range - N/S/H (H)(S15-S30)(N)

PropertyValue




Cutting Speed for: SMF240 AH9130 - 6790355
ISOMaterialsMaterial DesignationMaterial ConditionCutting Speed Recommendations (Vc)
P1Non-alloy steel and cast steel, free cutting steel <0.25%C.Annealed :12580-140 m/min
P2Non-alloy steel and cast steel, free cutting steel >=0.25%C.Annealed :19080-140 m/min
P3Non-alloy steel and cast steel, free cutting steel <0.55%C.Quench and tempered. :25080-140 m/min
P4Non-alloy steel and cast steel, free cutting steel >=0.55%C.Annealed :22080-140 m/min
P5Non-alloy steel and cast steel, free cutting steel >=0.55%C.Quenched & tempered. :30080-140 m/min
P6Low alloy & cast steel (less than 5% of alloying elements).Annealed :20070-120 m/min
P7Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :27570-120 m/min
P8Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :30040-90 m/min
P9Low alloy & cast steel (less than 5% of alloying elements).Quenched & tempered :35040-90 m/min
P10High alloyed steel, cast steel and tool steel.Annealed :20040-90 m/min
P11High alloyed steel, cast steel and tool steel.Quenched & tempered :32540-90 m/min
P12Stainless steel and cast steel.Ferritic/martensitic :20030-80 m/min
P13Stainless steel and cast steel.Martensitic :24030-80 m/min
M14Stainless steel and cast steel.Austenitic :18030-80 m/min
K15Grey cast iron (GG)Pearlitic/ferritic :18080-180 m/min
K16Grey cast iron (GG)Pearlitic/martensiti :26080-180 m/min
K17Nodular cast iron (GGG)Ferritic :16080-140 m/min
K18Nodular cast iron (GGG)Pearlitic :25080-140 m/min
K19Malleable cast iron.Ferritic :13080-140 m/min
K20Malleable cast iron.Pearlitic :23080-140 m/min
N21Aluminum-wrought alloy.Not cureable : 6080-220 m/min
N22Aluminum-wrought alloy.Cured :10080-220 m/min
N23Aluminum-cast, alloyed <12% Si.Not cureable : 7580-220 m/min
N24Aluminum-cast, alloyed.Cured : 9080-220 m/min
N25Aluminum-cast, alloyed >12% Si.High temperature :13080-220 m/min
N26Copper alloys >1% pb.Free cutting :11080-220 m/min
N27Copper alloys.Brass : 9080-220 m/min
N28Copper alloys.Electrolitic copper :10080-220 m/min
S31High temp. alloys Fe based.Annealed :20020-50 m/min
S32High temp. alloys Fe based.Cured :28020-50 m/min
S33High temp. alloys. Ni or Co based.Annealed :25020-50 m/min
S34High temp. alloys. Ni or Co based.Cured :35020-50 m/min
S35High temp. alloys. Ni or Co based.Castr :32020-50 m/min
S36Titanium Ti alloys.:31020-50 m/min
S37Titanium Ti alloys.Alpha+beta alloys cu :31020-50 m/min
H38Hardened steel.Hardened :56020-50 m/min
H39Hardened steel.Hardened :65420-50 m/min
H40Chilled cast iron.Cast :40020-50 m/min
H41Cast iron.Hardened :56020-50 m/min

Site Map:

External Turning  Internal Turning  Grooving & Parting  Threading  Milling  Holemaking  Boring  Tooling System 

Terms of Use and Legal Disclaimer   Privacy Statement   Privacy Settings
© 2024Tungaloy Corporation Manufacturer of Metalworking Tools (Tungaloy.co.jp) All Rights Reserved